X12MF / D2 /1.2379 / CR12MO1V1

Characteristics for grade Kh12MF (Х12МФ)

Brand: X12MF
Substitute: Kh6VF, Kh12F1, Kh12VM
Classification: Tool steel
Products offered by advertisers: No data
Application: profiling rollers of complex shapes, sections of body dies of complex shapes, complex hole-piercing dies when forming sheet metal, reference gears, rolling dies, dies, dies and punches of punching punched punches with a complex configuration of working parts, stamping of the active part of electrical machines.

Chemical composition in% for grade Х12МФ (Х12МФ)

GOST 5950-2000

C Si Mn Ni S P Cr Mo V Cu
1.45 - 1.65 0.1 - 0.4 0.15 - 0.45 up to 0.4 up to 0.03 up to 0.03 11 - 12.5 0.4 - 0.6 0.15 - 0.3 up to 0.3

Температура критических точек материала Х12МФ

Ac1 = 810 ,      Ac3(Acm) = 860 ,       Ar3(Arcm) = 780 ,       Ar1 = 760 ,       Mn = 225

Технологические свойства материала Х12МФ

        Свариваемость:     не применяется для сварных конструкций.
        Склонность к отпускной хрупкости:     склонна.
    Твердость   Х12МФ   после отжига ,             ГОСТ 5950-2000 HB 10 -1 = 255   МПа

Зарубежные аналоги материала Х12МФ

Внимание!   Указаны как точные, так и ближайшие аналоги.

США Германия Япония Франция Англия Евросоюз Италия
- DIN,WNr JIS AFNOR BS EN UNI
D2
T30402
1.2379
1.2601
X162CrMoV12
X165CrMoV12
Х155CrVMo12-1
SKD11 X160CrMoV12
Z160CDV12
BD2 X160CrMoV12-1 C165CrMoV12KU
X155CrVMo12-1KU
Испания Швеция Болгария Венгрия Польша Чехия Австрия
UNE SS BDS MSZ PN CSN ONORM
X160CrMoV12 2310 Ch12MF K8 NC11LV 19572 K105

Legend:

Weldability:
without Borders - welding is carried out without heating and without subsequent heat treatment
limited weldable - welding is possible when heated to 100-120 degrees. and subsequent heat treatment
difficult to weld - to obtain high-quality welded joints, additional operations are required: heating up to 200-300 degrees. when welding, heat treatment after welding - annealing